Characteristics and molding attention of electronic stamping parts
Release Time:
2023-05-26 10:39
Stamping parts factory to determine the meandering parts of the process plan that is to determine the multi-process meandering process placement and the layout of the mold for each process, to reasonably determine the meandering process plan, you must first master the commonly used meandering mold layout and working reason, and then according to the mold layout, working reason and characteristics of the determination of the process plan and the placement of the process.
Electronic stamping products in the daily processing has its strange characteristics:
1. Electronic stamping parts processing in the number of processes and the nature of the material, tensile height, tensile gateway, and pulling quite diameter, material thickness and other prerequisites;
2. Electronic stamping parts rinsing process with alkali rinsing, solvent rinsing, surfactant rinsing and other chemical rinsing method;
3. Electronic stamping parts plating and substrate adhesion is to manage the quality of plating products, the substrate material in the plating before, there will be a variety of surface dirt, such as (cutting fluid, lubricating fluid, polishing paste, etc.). The cleanliness of the surface of the substrate material simply affects the adhesion of the plating layer, and the surface of the sticky oil must be rinsed.
Electronic Stamping Products
Most of the electronic stamping parts are used in multi-effect digital or home appliance equipment, because the parts are relatively small, molding what we need to pay attention to?
1, electronic stamping parts forming status within the R circle should not be too large, because it itself in addition to plastic deformation will have elastic deformation, if the R is large then the rebound increases and can not manage to form the angle of consolidation;
2, forming punch arc should not be too small, if the punch forming angle is small, easy to scrape the outside of the material, common on soft materials is very low for double T, hard materials can not be less than 1.5-2T;
3, forming straight edge can not be too short, in order to ensure that the electronic stamping parts forming status and angle of consolidation of the relationship between the forming straight section despite the high, very low not less than 2T;
4, if forming and hole position is relatively close, in order to ensure that the hole is not easy to deform, but also to ensure the accuracy, although it should be formed in accordance with the relationship between the inner rounded angle r and plate thickness t (t < 2, 1 ≥ r + t; t ≥ 2, 1 ≥ r + 2t)
Related News
In accordance with our company motto, "Planning is implementation," we have built a relationship of trust with our customers since the establishment of Mori Die & Mold in 1977, based on careful planning and prompt action. "It is our desire to help our customers succeed, and it is also our company's success.
Plasess Plastics (ZhongShan) Co.,Ltd
Address: 1/3, 2/F, Building E, No. 21 Yanjiang Dongsan Road, Torch Development Zone, Zhongshan, Guangdong, China
Tel:0760-85314317
18925321803 ( Mr. Li )
Copyright © Plasess Plastics (ZhongShan) Co.,Ltd Business License